Manual Creep Tester

Manual Creep Tester per ASTM D3575-20

 

Schap Manual Creep Tester per ASTM D3575 provides constant compression creep testing. Creep testing is used to evaluate the long-term structural integrity and cushioning retention of; flexible open or closed-cell polyolefin foams, by measuring their time-dependent deformation under a steady static load. During this procedure, foam specimens are subjected to a constant compressive stress within a controlled laboratory environment for a specified duration of time. The creep tester uses a 200 mm platen to compress your foam samples. Additional stock and custom platen sizes are available.

Available weights:

2.5 lb.

SKU 710R1001

5 lb.

SKU 710R1002

10 lb.

SKU 710R1003

20 lb.

SKU 710R1004

 

12″ x 12″ base x 33.25″ Tall

26 lbs

 

304.8 mm x 304.8 mm base x 844.5 mm Tall

11.8 kg

 

Weight 11.8 kg
Dimensions 844.5 × 304.8 × 304.8 mm